Welds that don't flow well
 

Welds that don't flow well

Started by Zephod, June 23, 2017, 06:07:16 PM

Previous topic - Next topic

Zephod

I've been doing some butt welding with 6011 rods. They should flow more consistently than they are. The amperage is right. I'm not moving the rod too fast. I see a very nice weld.

When I grind the weld down flush there are places under the weld where the rod has not flowed into the crevices well. It's the lack of consistency that puzzles me. It all should be fine. Right rod, right amperage, right speed. Surfaces are bare steel.



Sent from my iPad using Tapatalk
Carpenter 3800 1994 on a Navistar 1994 chassis with a DT466 and alinson transmission.

krcevs

It looks like your material was dirty prior to welding. Are you grinding the surface to get clean metal first? I would also suggest some anti splatter spray as well. Keeps the slag splatter down quite a bit.

Ken
Kim and Ken Carpenter
GMC PD4107-1121
GMC PD4107=1180
Berthoud CO

"Here hold my beer!"

luvrbus

I never heard of anti splatter spray for a stick rod does it work on a stick rod I never tried it before except on my Mig